pH Evaluation over a Period of 6 months of Two-bottle Water-based Self-etching Primers: An In Vitro Study

Nicola De Angelis, Nicolò Di Tullio

Keywords : Adhesive, pH, Primers, Self-etching

Citation Information : De Angelis N, Di Tullio N. pH Evaluation over a Period of 6 months of Two-bottle Water-based Self-etching Primers: An In Vitro Study. J Contemp Dent Pract 2021; 22 (8):856-859.

DOI: 10.5005/jp-journals-10024-3172

License: CC BY-NC 4.0

Published Online: 09-11-2021

Copyright Statement:  Copyright © 2021; The Author(s).


Abstract

Aim and objective: The objective of this study was to monitor the pH stability over a period of 6 months of two-bottle self-etching (SE) primers. Materials and methods: Four commercially available two-bottle SE primer solutions, Adhese SE (Ivoclar Vivadent; Schaan, Liechtenstein), Clearfil SE (Kuraray; Tokyo, Japan), Contax Primer (DMG; Hamburg, Germany), and Enabond SE (Micerium; Avegno (Ge), Italy), containing water as the main solvent were selected. The pH values during a 6-month storage period at intermittent temperature were daily measured by means of a microprocessor-based pH/temperature meter and hence recorded, tabulated, and analyzed. Results: The mean values of overall pH measurements and standard deviation for Adhese SE, Clearfil SE, Contax Primer, and Enabond SE are, respectively, 1.70 (±0.01), 1.72 (±0.01), 1.20 (±0.01), 1.80 (±0.01). One-way ANOVA did not detect any significant change of the mean pH values of all measurements over time. Conclusion: The conventional 6-months storage did not affect the pH values of the water-containing primers of two-bottle SE adhesives. Clinical significance: This study provides evidence that conventional storage under adequate conditions did not affect the pH values of the water-containing primers of two-bottle SE adhesives with different monomer formulations. Clinicians may rely on the known pH value of the selected SE adhesive during shelf-life.


HTML PDF Share
  1. Tay FR, Pashley DH. Aggressiveness of contemporary self-etching systems. I: depth of penetration beyond dentin smear layers. Dent Mater 2001;17(4):296–308. DOI: 10.1016/s0109-5641(00)00087-7.
  2. Van Meerbeek B, Yoshihara K, Yoshida Y, et al. State of the art of self-etch adhesives. Dent Mater 2011;27(1):17–28. DOI: 10.1016/j.dental.2010.10.023.
  3. Van Meerbeek B, De Munck J, Yoshida Y, et al. Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges. Oper Dent 2003;28(3):215–235. PMID: 12760693.
  4. Moszner N, Salz U, Zimmermann J. Chemical aspects of self-etching enamel-dentin adhesives: a systematic review. Dent Mater 2005;21(10):895–910. DOI: 10.1016/j.dental.2005.05.001.
  5. Salz U, Mücke A, Zimmermann J, et al. pKa value and buffering capacity of acidic monomers commonly used in self-etching primers. J Adhes Dent 2006;8(3):143–150. PMID: 16830660.
  6. Iwasa M, Tsubota K, Shimamura Y, et al. pH changes upon mixing of single-step self-etching adhesives with powdered dentin. J Adhes Dent 2011;13(3):207–212. DOI: 10.3290/j.jad.a19240.
  7. Van Landuyt KL, Snauwaert J, De Munck J, et al. Systematic review of the chemical composition of contemporary dental adhesives. Biomaterials 2007;28(26):3757–3785. DOI: 10.1016/j.biomaterials.2007.04.044.
  8. Koshiro K, Sidhu SK, Inoue S, et al. New concept of resin-dentin interfacial adhesion: the nanointeraction zone. J Biomed Mater Res B Appl Biomater 2006;77(2):401–408. DOI: 10.1002/jbm.b.30450.
  9. Nishiyama N, Suzuki K, Yoshida H, et al. Hydrolytic stability of methacrylamide in acidic aqueous solution. Biomaterials 2004;25(6):965–969. DOI: 10.1016/s0142-9612(03)00616-1.
  10. Salz U, Zimmermann J, Zeuner F, et al. Hydrolytic stability of self-etching adhesive systems. J Adhes Dent 2005;7(2):107–116. PMID: 16052759.
  11. Lima GdaS, Ogliari FA, da Silva EO, et al. Influence of water concentration in an experimental self-etching primer on the bond strength to dentin. J Adhes Dent 2008;10(3):167–172. PMID: 18652264.
  12. Moura SK, Pelizzaro A, Dal Bianco K, et al. Does the acidity of self-etching primers affect bond strength and surface morphology of enamel? J Adhes Dent 2006;8(2):75–83. PMID: 16708718.
  13. Breschi L, Gobbi P, Mazzotti G, et al. High resolution SEM evaluation of dentin etched with maleic and citric acid. Dent Mater 2002;18(1):26–35. DOI: 10.1016/s0109-5641(01)00017-3.
  14. Kenshima S, Francci C, Reis A, et al. Conditioning effect on dentin, resin tags and hybrid layer of different acidity self-etch adhesives applied to thick and thin smear layer. J Dent 2006;34(10):775–783. DOI: 10.1016/j.jdent.2006.03.001.
  15. Nishiyama N, Tay FR, Fujita K, et al. Hydrolysis of functional monomers in a single-bottle self-etching primer--correlation of 13C NMR and TEM findings. J Dent Res 2006;85(5):422–426. DOI: 10.1177/154405910608500505.
  16. Cheng KL, Zhu DM. On calibration of pH meters. Sensors 2005;5(4):209–219. DOI: 10.3390/s5040209.
  17. Meinrath G, Spitzer P. Uncertainties in determination of pH. Microchim Acta 2000;13(3–4):155–168. DOI: 10.1007/s006040070005.
  18. Pashley DH, Carvalho RM, Tay FR, et al. Solvation of dried dentin matrix by water and other polar solvents. Am J Dent 2002;15(2):97–102. PMID: 12092999.
PDF Share
PDF Share

© Jaypee Brothers Medical Publishers (P) LTD.