CASE REPORT

New Single-bottle Ceramic Primer: 6-month Case Report and Laboratory Performance

Fabiana SF Siqueira, Rodrigo S Alessi, Andres FM Cardenas, Carlos Kose, Shelon C Souza Pinto, Alessandro D Loguercio, João C Gomes

Citation Information : Siqueira FS, Alessi RS, Cardenas AF, Kose C, Pinto SC, Loguercio AD, Gomes JC. New Single-bottle Ceramic Primer: 6-month Case Report and Laboratory Performance. J Contemp Dent Pract 2016; 17 (12):1033-1039.

DOI: 10.5005/jp-journals-10024-1977

Published Online: 01-04-2017

Copyright Statement:  Copyright © 2016; The Author(s).


Abstract

Introduction

This article presents a 6-month case report and an in vitro evaluation of the performance of the new self-etching glass-ceramic monobond etch and prime (MEP) when applied in a lithium disilicate (LD). The MEP contains in the same bottle, along with acid conditioner and silanes. This simplifies the bonding procedures by reducing not only the number of steps, but also the working time. A 42-year-old female patient sought for esthetic treatment, and the main complaint was the darkened appearance of the upper lateral incisor. The esthetic treatment includes dental bleaching and gingivectomy, all-ceramic zirconia crowns, and all-ceramic crown and laminate veneer LD. After 6 months of esthetic treatment, marginal staining, gap, or chip fracturing damaging margins after sharp explorer in the margins was not observed. Furthermore, the inferior etching pattern of MEP was compared with traditional hydrofluoric acid (HF) conditioning. The microshear bond strength to the intaglio surface of LD was statistically similar when HF was compared with MEP. This new self-etching glass-ceramic showed good in vitro and 6 months clinical results in this case report. Future long-term clinical studies with more clinical case need to be done to confirm the performance of the use of this new conditioner.

Clinical significance

The use of a new self-etching glassceramic showed a good in vitro and 6 months clinical results. This new product can be an easy, simple, and alternative approach for esthetics bonding procedure.

How to cite this article

Siqueira FSF, Alessi RS, Cardenas AFM, Kose C, Souza Pinto SC, Bandeca MC, Loguercio AD, Gomes JC. New Single-bottle Ceramic Primer: 6-month Case Report and Laboratory Performance. J Contemp Dent Pract 2016; 17(12):1033-1039.


PDF Share
  1. Effect of different ceramic surface treatments on resin microtensile bond strength. J Prosthodont 2004 Mar;13(1):28-35.
  2. Effect of different etching periods on the bond strength of a composite resin to a machinable porcelain. J Dent 1998 Jan;26(1):53-58.
  3. Molecular orientation of silane at the surface of colloidal silica. J Dent Res 1993 Jun;72(6):1050-1054.
  4. The influence of cement lute, thermocycling and surface preparation on the strength of a porcelain laminate veneering material. Dent Mater 2004 Mar;20(3):286-292.
  5. The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative material. Dent Mater 2007 Apr;23(4):461-468.
  6. Effect of ceramic surface treatment on tensile bond strength to a resin cement. Int J Prosthodont 2002 May-Jun;15(3):248-253.
  7. Hydrofluoric acid: a review of toxicity. J Emerg Med 1992 Mar-Apr;10(2):163-168.
  8. Possible hazardous effects of hydrofluoric acid and recommendations for treatment approach: a review. Clin Oral Invest 2012 Feb;16(1):15-23.
  9. Evaluation of alternative intra-oral repair techniques for fractured ceramic-fused-to-metal restorations. J Oral Rehabil 2003 Feb;30(2):194-203.
  10. Bond Strength of Resin Cement to Lithium Disilicate with Pre-treatments. J Dent Res 2016;95(Special issue A):Abstract 569.
  11. Stability of Silane to Lithium Disilicate in Extreme Environmental Conditions. J Dent Res 2016;95(Special issue A): Abstract 571.
  12. Shear Bond Strength of Ceramic Primers with Lithium Disilicate. J Dent Res 2016;95(Special Issue A):Abstract 1083.
  13. Effect of Storage on Shear-bond Strength of Self-Etch Ceramic Primer. J Dent Res. 2016;95(Special issue A):Abstract 1067.
  14. Use of a direct anatomic post in a flared root canal: a three-year follow-up. Oper Dent 2016 Jan-Feb;41(1):E23-28.
  15. Four-year follow-up of a direct anatomical fiber post and esthetic procedures: a case report. Oper Dent 2016 Jul-Aug;41(4):363-369.
  16. Laboratory performance of universal adhesive systems for luting CAD/CAM restorative materials. J Adhes Dent 2016;18(4):331-340.
  17. The effect of the loading method and cross-head speed on resin-dentin microshear bond strength. Int J Adhes Adhes 2014 Apr;50:136-141.
  18. Micro-shear bond strength of dual-cured resin cement to glass ceramics. Dent Mater 2002 Jul;18(5):380-388.
  19. Monobond Etch & Prime:2015; 2015. Available from: http://www.ivoclarvivadent.com/en/bonding-agentsluting-composites-to-restorations/monobond-etch-and-prime. [Last cited on April 18, 2016].
  20. Effect of surface acid etching on the biaxial flexural strength of two hot-pressed glass ceramics. J Prosthodont 2008 Jul;17(5):415-419.
  21. Effect of etching time and resin bond on the flexural strength of IPS e.max Press glass ceramic. Dent Mater 2014 Dec;30(12):e330-336.
  22. Effect of hydrofluoric acid etching duration on the roughness and flexural strength of a lithium disilicate-based glass ceramic. Braz Dent J 2011;22(1):45-50.
  23. Technique-sensitivity of contemporary adhesives. Dent Mater J 2005 Mar;24(1):1-13.
  24. New developments in dental adhesion. Dent Clin North Am 2007 Apr;51(2):333-357, viii.
  25. The effects of different shades of resin luting cement on the color of ceramic veneers. Dent Mater J 2012;31(3):354-361.
  26. Porcelain veneers as an alternative for the esthetic treatment of stained anterior teeth: clinical report. Quintessence Int 2005 Mar;36(3):191-196.
  27. Esthetic rehabilitation of worn anterior teeth with thin porcelain laminate veneers. Eur J Esthet Dent 2011 Autumn;6(3):298-313.
  28. Porcelain veneers as an alternative for esthetic treatment: clinical report. Oper Dent 2013 Sep-Oct;38(5):459-466.
  29. Materials for chairside CAD/CAM-produced restorations. J Am Dent Assoc 2006 Sep;137 Suppl:14S-21S.
  30. Clinical performance of porcelain laminate veneers for up to 20 years. Int J Prosthodont 2012 Jan-Feb;25(1):79-85.
  31. Survival rates for porcelain laminate veneers with special reference to the effect of preparation in dentin: a literature review. J Esthet Restor Dent 2012 Aug;24(4):257-265.
  32. Influence of cement shade and water storage on the final color of leucite-reinforced ceramics. Oper Dent 2008 Jul-Aug;33(4):386-391.
PDF Share
PDF Share

© Jaypee Brothers Medical Publishers (P) LTD.