RESEARCH ARTICLE

Influence of Dentin Deproteinization on Bonding Degradation: 1-year Results

Carlos Rocha Gomes Torres, Eduardo Bresciani, César R Pucci, Natália R Barbosa, Karen CK Yui, Maria Filomena RL Huhtala, Daphne C Barcellos

Citation Information : Torres CR, Bresciani E, Pucci CR, Barbosa NR, Yui KC, Huhtala MF, Barcellos DC. Influence of Dentin Deproteinization on Bonding Degradation: 1-year Results. J Contemp Dent Pract 2016; 17 (12):985-989.

DOI: 10.5005/jp-journals-10024-1968

Published Online: 01-05-2017

Copyright Statement:  Copyright © 2016; The Author(s).


Abstract

Introduction

The decalcification protocol of dentin surface with sodium hypochlorite removes the exposed collagen fibrils and could improve the longevity of the bonding interface. This study evaluated the influence of collagen removal with 10% sodium hypochlorite (10% NaOCl) on the longitudinal shear bond strength (SBS) of adhesives to dentin.

Materials and methods

Seventy-two extracted human molars were sectioned and the buccal and lingual surfaces were flattened and acid etched with 37% phosphoric acid for 15 seconds. The specimens were divided into six groups (n = 12 teeth – 24 sections), according to adhesive and collagen removal protocol: group 1: UNO Dentastic; group 2: Prime and Bond NT; group 3: Single Bond; group 4: 10% NaOCl + UNO Dentastic; group 5: 10% NaOCl + Prime and Bond NT; group 6: 10% NaOCl + Single Bond. Composite Z100 buildup was prepared, and the SBS test was assessed after 24 hours and 1 year. Data were submitted to three-way analysis of variance (ANOVA) and Tukey tests (p < 0.05).

Results

The mean values (MPa) were for 24 hours: G1: 22.45B; G2: 7.90DE; G3: 12.56CD; G4: 19.85BC; G5: 33.73A; G6: 20.77B; and for 1 year: G1: 2.43E; G2: 2.26E; G3: 4.3DE; G4: 18.79BC; G5: 26.49AB; G6: 22.73B.

Conclusion

Dentin deproteinization treatment with 10% NaOCI influenced the SBS compared with conventional treatment. The negative influence on SBS detected for conventional groups at 1-year interval was not detected for deproteinized groups.

Clinical relevance

The longevity of hybrid layer is critical due to the hydrolysis process at the adhesive interface over time. The use of 10% NaOCl deproteinization protocol might improve the longevity of bonding in adhesive restorations.

How to cite this article

Pucci CR, Barbosa NR, Bresciani E, Yui KCK, Huhtala MFRL, Barcellos DC, Torres CRG. Influence of Dentin Deproteinization on Bonding Degradation: 1-year Results. J Contemp Dent Pract 2016;17(12):985-989.


PDF Share
  1. Aging affects two modes of nanoleakage expression in bonded dentin. J Dent Res 2003 Jul;82(7):537-541.
  2. Comparative SEM and TEM observations of nanoleakage within the hybrid layer. Oper Dent 1995 Jul-Aug;20(4):160-167.
  3. How to increase the durability of resin-dentin bonds. Compend Contin Educ Dent 2011 Sep;32(7):60-64,66.
  4. Microporous dentin zone beneath resin-impregnated layer. Oper Dent 1994 Mar-Apr;19(2):59-64.
  5. Dentine permeability and dentine adhesion. J Dent 1997 Sep;25(5):355-372.
  6. Bonding efficacy of an acetone/based etch-and-rinse adhesive after dentin deproteinization. Med Oral Patol Oral Cir Bucal 2012 Jul;17(4):e649-654.
  7. Effect of a sodium hypochlorite gel on dentin bonding. Dent Mater 2000 Sep;16(5):311-323.
  8. Influence of NaOCl deproteinization on shear bond strength in function of dentin depth. Am J Dent 2002 Aug;15(4):252-255.
  9. An ultramorphological characterization of collagen-depleted etched dentin. Am J Dent 1999 Oct;12(5):250-255.
  10. Changes in bovine dentin mineral with sodium hypochlorite treatment. J Dent Res 1988 Sep;67(9):1229-1234.
  11. The overwet phenomenon: an optical, micromorphological study of surface moisture in the acid-conditioned, resin-dentin interface. Am J Dent 1996 Feb;9(1):43-48.
  12. Longitudinal bond strength evaluation using the deproteinized dentin technique. Gen Dent 2009 Jul-Aug;57(4):328-333; quiz 334-5.
  13. Short- and long-term in vitro study of the bonding of eight commercial adhesives to normal and deproteinized dentin. Acta Odontol Scand 2006 Aug;64(4):237-243.
  14. Durable bonds at the adjesive/dentin interface: an impossible mission or simply a moving target? Braz Dent Sci 2012 Jan-Mar;15(1):4-18.
  15. The chemistry of adhesive agents. Oper Dent Suppl 1992; Suppl 5:32-43.
  16. Wet or dry, normal or deproteinized dentin surfaces as substrate for dentin adhesives. Acta Odontol Scand 2002 Jan;60(1):60-64.
  17. A nanoleakage perspective on bonding to oxidized dentin. J Dent Res 2002 Sep;81(9):628-632.
  18. Reversal of compromised bonding to oxidized etched dentin. J Dent Res 2001 Oct;80(10):1919-1924.
  19. Solvent content and dentin bond strengths using water-wet, ethanol-wet and deproteinization bonding techniques. Acta Odontol Scand 2013 May-Jul;71(3-4):710-715.
  20. Effect of dentin pretreatment with mild acidic HOCl solution on microtensile bond strength and surface pH. J Dent 2010 Mar;38(3):261-268.
  21. A critical review of the durability of adhesion to tooth tissue: methods and results. J Dent Res 2005 Feb;84(2):118-132.
  22. Dynamic contact angle and spreading rate measurements for the characterization of the effect of dentin surface treatments. J Colloid Interf Sci 2003 Jul;263(1):162-169.
PDF Share
PDF Share

© Jaypee Brothers Medical Publishers (P) LTD.